A thermal outgassing method (t.o.m.) To measure the hydrogen diffusion coefficients in austenitic, austeno-ferritic and ferritic–perlitic steels
1998
·
F. Iacoviello
, J. Galland
, et al.
·
Corrosion Science
·
36
Hydrogen embrittlement in the duplex stainless steel Z2CND2205 hydrogen-charged at 200°C
1997
·
F. Iacoviello
, M. Habashi
, et al.
·
Materials Science and Engineering A
·
30
Quantitative measurements of the degree of exfoliation on aluminium alloys
1993
·
M. Habashi
, E. Bonte
, et al.
·
Corrosion Science
·
13
Comportement mécanique de l'acier inoxydable martensitique 17-4 PH en corrosion sous contrainte et à la fragilisation par l'hydrogéne environnemental
1999
·
F ELHILALI
, M HABASHI
, et al.
·
Annales de Chimie Science des Matériaux
·
11
HYDROGEN EMBRITTLEMENT IN Al-Li-Cu-Mg ALLOYS (8090-T651)
1987
·
F. BINSFELD
, M. HABASHI
, et al.
·
Le Journal de Physique Colloques
·
9
High-Strength Steels with Improved Sulfide Stress Cracking Resistance
1986
·
A. Chavane
, M. Habashi
, et al.
·
CORROSION
·
6
Corrélation entre la perméation électrochimique et la fragilisation par l'hydrogène de l'acier inoxydable 17-4 PH : rôle de la microstructure
1998
·
F. El Hilali
, M. Jérôme
, et al.
·
Matériaux & Techniques
·
4
Mechanisms of Hydrogen Embrittlement During Low Cycle-Fatigue in Metastable Austenite
1992
·
M. Labidi
, M. Habashi
, et al.
·
Springer eBooks
·
3
CORRELATION BETWEEN LONG TIME AND SHORT TIME TESTS TO DETECT PITTING AND EXFOLIATION CORROSION IN Al-Li (8090) ALLOYS
1987
·
J. GARCIA
, P. PONTHIAUX
, et al.
·
Le Journal de Physique Colloques
·
3
Hydrogen Damage Detection in 304l and 321 Austenitic Stainless Steels With and Without Hydrogen Dislocations Interactions
1984
·
P. Huwart
, M. Habashi
, et al.
·
Elsevier eBooks
·
2
Correlation Between Apparent Toughness Ka and Charpy Impact Energy in High and Low Strength Steels
1984
·
M. Habashi
, M. Tvrdy
, et al.
·
Elsevier eBooks
·
2
Relationships between KIC and CVN at the Lower Shelf of the Transition Curve CVN-T
2015
·
M. Habashi
, M. Tvrdy
·
Journal of Materials Science and Engineering A
·
1
Application of local approach of fracture in a pearlitic steel cathodically hydrogenated
1990
·
A. FONTAINE
, S. JEUNEHOMME
, et al.
·
Gruppo Italiano Frattura Digital Repository (Gruppo Italiano Frattura)
·
1
EFFECT OF GRAIN SIZE ON THRESHOLD VALUE KISH IN AGEING MARTENSITIC Fe-Ni-C ALLOY CATHODICALLY HYDROGENATED AT ROOM TEMPERATURE
1982
·
M. Tvrdy
, M. Habashi
, et al.
·
Elsevier eBooks
·
1
An attempt to correlate the change of the swept area (∆A/b2) by mobile dislocations with the mechanism of the fatigue crack propagation rate (da/dN) in environmental hydrogen: Application in Inconel 690
2017
·
Xinghong Luo
, Mahmoud Habashi
·
Materials Science and Engineering A
A thermal outgassing method (T.O.M.) to measure the hydrogen coefficient of diffusion in austenitic and austeno-ferritic steels
1998
·
IACOVIELLO, Francesco
, J. GALLAND
, et al.
·
Archivio Istituzionale della Ricerca - Università degli Studi di Cassino
Effect of hydrogen embrittlement during low-cycle fatigue in metastable austenite
1997
·
May Labidi
, M. Habashi
, et al.
Recupero delle proprieta meccaniche di un acciaio duplex austeno-ferritico Z2CND2205 dopo infragilimento da idrogeno
1996
·
IACOVIELLO, Francesco
, M. Habashi
·
Gruppo Italiano Frattura Digital Repository (Gruppo Italiano Frattura)
Internal Hydrogen Embrittlement at 300°C in Nickel Base Alloys 690 and 800
1994
·
I. Lenartova
, M. Habashi
, et al.
Hydrogen Embrittlement in Duplex Steel Tempered between 200°C and 1050°C and Cathodically Charged at 200°C
1994
·
F. Iacoviello
, M. Habashi
, et al.
Local Approach of Fracture in a Tempered Martensitic Steel Cathodically Hydrogenated at High pH
1994
·
R.P. Hu
, M. Habashi
, et al.
Etude de la résistance à la fissuration par l’hydrogène des joints soudés d’aciers de construction modernes.
1994
·
A. Felix-Henry
, T. Maurickx
, et al.
·
Revue de Métallurgie
Comparison between Environmental Hydrogen Crack Growth Rate Measurements by Applying Constant Load, Constant C.T.O.D. and Constant C.T.O.D. Rate.
1994
·
E. Bonte
, M. Habashi
, et al.
·
NACE CORROSION Conference
Hydrogen Embrittlement on α-Iron in High Alkaline Environment
1994
·
R. Hu
, M. Habashi
, et al.
·
NACE CORROSION Conference
Morfologie di infragilimento da idrogeno in un acciaio austeno-ferritico
1994
·
IACOVIELLO, Francesco
, M. Cavallini
, et al.
·
Archivio Istituzionale della Ricerca - Università degli Studi di Cassino
Show more works
View as search
Works count:
43
Citation count:
122
H-index:
6
I10-index:
4
Year
Topic
Type