Pemanfaatan Hasil Hidrolisis Dan AlkoksilasiDengan Gliserol Dari Epoksida MinyakKemiri Sebagai Sumber Poliol UntukPembuatan Poliuretan
Year: 2010
Type: article
Abstract: Polyurethane can be produced by polymerisation of diisocyanate with polyol. Polyol can be produced by oxidation of unsaturated fatty acid with peracid followed by hydrolysis or alkoxylation of cyclic epoxyde..The purpose of this research was to synthesize polyurethane using unsaturated fatty acid from candlenut oil as the raw material to produce polyol. Materials and reagents used were candlenut oil’s, performic acid obtained from reaction of formic acid and hydrogen peroxide, toluene diisocyanate (TDI), glycerol and dichloromethane as a solvent. This research was conducted through epoxidation of unsaturated fatty acid followed by hydrolysis (PHHEM) and alkoxylation with glycerol (PHAGEM) in propanone to obtain two kinds of polyol derivatives from candlenut oil. Synthesis of polyurethane was carried out by reacting toluene diisosyanate with various ratio of polyol. Reaction was carried out by reflux with dichloromethane as a solvent. The product was characterized with saveral parameters such as morphology characterization, gel content, tensile strength, elasticity and also functional group characterization with FT-IR spectroscopy. The result of FT-IR spectroscopy analysis towards the yield of the polymerization produced spectrum which could indicate that the yield of the reaction is polyurethane with the accurance of vibration peak on the wave numbers of 3400- 3300 cm-1, 1730- 1710, 1640-1600 and 1590- 1540 cm-1, proved that there was a urethane group (-NHCOO-) present. The highest value of tensile strength (σt) on obtained polyurethane was on the polyol/TDI ratio = 7/3 (v/v) using PHHEM = 6.0 MPa ( elasticity,ε = 47.54%, gel content, Q = 81.77%, adhesive), PHAGEM = 7.95 MPa (ε = 36.33%, Q = 80.63%, adhesive) and PEG – 1000 = 9.15 MPa (ε = 28.79%, Q = 98.31%. foam). The highest Q could be found with the use of PHHEM on the 5/5 (v/v) ratio = 97.72% (σt = 0.35, ε = 9.57. hard), PHAGEM on 4/6 (v/v) ratio = 97.52% (σt = 0.18, ε = 9.52%, hard) and PEG – 1000 on 6/4 (v/v) ratio = 98,68% (σt = 5.57 MPa, ε = 41.06%, foam). Furthermore, the result of this research could give information that by using the mixture of PHHEM or PHAGEM polyol with PEG- 1000 could increase, both the value of tensile strength or percentage of gel content of formed polyurethane.
Author: Mimpin Ginting
Language: Indonesian
Subfield: Polymers and Plastics
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W1007339576