Теплоемкость, тепловое расширение и калорические эффекты в композите сегнетоэлектрик-ферромагнетик 0. 82(PbTi O. 3) 0. 18(Lа 0. 7рb 0. 3мn0 3)
Year: 2013
Type: article
Abstract: Heat capacity and thermal expansion measurements on ceramic composite 0,82(PbTi0 3) 0,18(La 0,7Pb 0,3Mn0 3) were performed at a wide temperature range. The cross impact of ferroelectric and ferromagnetic components on electro-, magnetoand barocaloric efficiency of the material was studied in phase transition regions.
Source: Siberian Aerospace Journal
Language: Russian
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W1017923201