Work

Study of Corrosion and Corrosion Inhibition of Chromate and Chromate-Free Primers

Year: 2012
Type: article
Abstract: Chromate and chromate-free primers were characterized in this study.For chromate primer examined, PPG EWEDA 144A (Pittsburgh Plate Glass Company), SrCrO 4 was the active inhibitor.The three chromate-free primers examined were Deft 02GN084, Hentzen 16708 TEP and Sicopoxy 577-630.In the Deft product, the active inhibitor was PrO/ Pr(OH) 3 .CaSiO 3 was the active inhibitor for Hentzen 16708 TEP and BaSO 4 for Sicopoxy 577-630.How each pigment reacted within its coating environment during exposure was an object of study and primers coatings were characterized by several techniques.Focused ion beam (FIB) milling was used to prepare cross sections for energy dispersive x-ray analysis (EDX) to identify pigments and inhibitors derived from them.A Matlab TM program was developed to analyze the resulting EDX maps to characterize the dispersion of elements in inhibitor ions produced by pigment dissolution during exposure.Pigment characteristics and pigment dissolution varied widely from primer to primer.Chromate pigments were present in high volume fractions in chromated primers.As a result pigment particles were in close proximity to one other and touching in 2D sections.In the chromate-free primers, inhibitor pigment particles were present in much lower volume fractions and were far away from each other.To quantify the protectiveness of chromate and chromate-free coatings systems in standard exposure testing on mixed metal structures, optical profilometry was used on DEDICATION For all my loving family who support me back at my home country, especially my parents and my sister.
Author: Longfei Li
Language: English
Open Access status: green
OpenAlex ID: W102020155
FWCI: 0.23
Cites: 45
Cited by: 3
Related to: 10