Abstract: Poor hermeticity performance was observed for Al{sub 2}O{sub 3}-Al{sub 2}O{sub 3} ceramic-ceramic joints having a Kovar{trademark} alloy interlayer. The active Ag-Cu-Ti filler metal was used to braze the substrates together. The Ti active element was scavenged from the filler metal by the formation of a (Fe, Ni, Co){sub x}Ti phase (x= 2-3) that prevented development of a continuous Ti{sub x}O{sub y} layer at the filler metal/Al{sub 2}O{sub 3} interface. Altering the process parameters did not circumvent the scavenging of Ti. Molybdenum barrier layers 1000, 2500, or 5000 {angstrom} thick on the Kovar{trademark} surfaces successfully allowed Ti{sub x}O{sub y} formation at the filler metal/Al{sub 2}O{sub 3} interface and hermetic joints. The problems with the Ag-Cu-Ti filler metal for Kovar{trademark}/Al{sub 2}O{sub 3} braze joints led to the evaluation of a Ag-Cu-Zr filler metal. The Zr (active element) in Ag-Cu-Zr filler metal was not susceptible to the scavenging problem.
Language: English
Open Access status: green
OpenAlex ID: W1483553364
FWCI:
Cites: 6
Cited by: 3
Related to: 10