Work

Mekani̇k Alaşimlama İle Üreti̇lmi̇ş Çi̇nko-alümi̇nyum (za) Alaşimlarinin Kuru Sürtünmeli̇ Aşinma Davranişlarinin İncelenmesi̇

Year: 2014
Type: article
Abstract: ZA alloy powders having different compositions were prepared by mechanical alloying in a spex mill. The mechanical alloying was applied 5 to 8 h and the ball to powder weight ratio was kept at 10:1 by weight. The mechanical milled/alloyed powders were warm-compacted at 320 °C and were sintered at the same temperature for 2 h. After the sintering process, the dry sliding wear test of the ZA alloys were conducted on a pin on disc wear testing machine. The wear load, the sliding speed and total sliding distance were sustained at 10 N, 1 m/s and 600 m respectively for all specimens. The Vickers hardness values of the ZA alloys varied from ~78 HV to ~145 HV depending on the increase in Aluminum content; however these values were steady by increasing milling time. It was seen that the wear volume rate and the sliding coefficient decreased as a consequence of increasing Aluminum content and hardness
Institution: Gazi University
Language: Turkish
Open Access status: diamond
OpenAlex ID: W1582962675
FWCI:
Cites: 10
Cited by: 1
Related to: 9