Work

Long-term aging of type 308 stainless steel welds: Effects on properties and microstructure

Year: 1994
Type: article
Abstract: Multipass gas tungsten arc welds with type 308 stainless steel filler metal in type 304L base plate have been aged at 400, 475, or 550{degrees}C for times up to 5,000 h. The changes in mechanical properties as a result of these agings have been followed with tensile, impact, and fracture toughness testing, using subsize tensile, half-size Charpy, and 0.45T compact specimens, respectively. The changes in the microstructure were evaluated with optical and transmission electron microscopy. Relatively little change was observed in the tensile properties for any of the aging treatments, but significant embrittlement was observed in the impact and fracture toughness testing. The transition temperatures increased rapidly for aging at 475 or 550{degrees}C, and more slowly for aging at 400{degrees}C. The upper-shelf energies and the fracture toughness showed similar responses, with only a small decrease for 400{degrees}C aging, but much greater and rapid decreases with aging at 475 or 550{degrees}C. Aging at 400 or 475{degrees}C resulted in the spinodal decomposition of the ferrite phase in the weld metal into iron-rich alpha and chromium-enriched alpha prime. In addition, at 475{degrees}C G-phase precipitates formed homogeneously in the ferrite and also at dislocations. At 550{degrees}C carbides formed and grew at the ferrite-austenite interfaces, and some ferrite transformed to sigma phase. These changes must all be considered in determining the effect of aging on the fracture properties.
Language: English
Open Access status: green
Award: G361195141
OpenAlex ID: W165379751
FWCI:
Cites:
Cited by: 1
Related to: 10