Year: 1993
Type: article
Abstract: Ti{sub 3}Al has very attractive properties such as low density and high temperature mechanical strength for elevated temperature structural applications. Its major drawback however, is poor oxidation resistance at temperatures above 600{degrees}C. Potential use of Ti{sub 3}Al in high temperature applications depends on its protection from excessive oxidation. To this effect, Al{sub 2}O{sub 3} and Al{sub 3}Ti were selected as coating materials chemically compatible with Ti{sub 3}Al. Al{sub 2}O{sub 3} acts as a protective layer on the surface of Ti{sub 3}Al and is impervious to oxygen diffusion. Al{sub 3}Ti is resistant to high temperatures and also protects the Ti{sub 3}Al substrate by forming an oxide layer consisting primarily of Al{sub 2}O{sub 3}. In this study, Al{sub 2}O{sub 3} was plasma sprayed onto the surface of Ti{sub 3}Al, while the Al{sub 3}Ti was applied by laser melting. Effectiveness of the coatings were investigated after 10 hours of cyclic oxidation.
Language: English
Subfield: Mechanical Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W173244106