Year: 2002
Type: conference-paper
Abstract: A program on fireside corrosion is being conducted at Argonne National Laboratory to evaluate the performance of several structural alloys in the presence of mixtures of synthetic coal ash, alkali sulfates, and alkali chlorides. Candidate alloys are also exposed in a small-scale coal-fired combustor at the National Energy Technology Laboratory in Pittsburgh. Experiments in the present program, which addresses the effects of deposit chemistry, temperature, and alloy chemistry on the corrosion response of alloys, were conducted at temperatures in the range of 575-800 C for time periods up to {approx}1850 h. Alloys selected for the study included HR3C, 310TaN, HR120, SAVE 25, NF709, modified 800, 347HFG, and HCM12A. In addition, 800H clad with Alloy 671 was included in several of the exposures. Data were obtained on weight change, scale thickness, internal penetration, microstructural characteristics of corrosion products, mechanical integrity, and cracking of scales. Results showed that relationship of corrosion rates to temperature followed a bell-shaped curve, with peak rates at {approx}725 C, but the rate itself was dependent on the alloy chemistry. Several alloys showed acceptable rates in the sulfate-containing coal-ash environment; but NaCl in the deposit led to catastrophic corrosion at 650 and 800 C.
Authors: K. Natesan, A. Purohit, D.L. Rink
Institution: Argonne National Laboratory
Language: English
Subfield: Surfaces, Coatings and Films
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
Award: G2123841078
OpenAlex ID: W189978014