PREPARATION AND PROPERTIES OF ION BEAM DEPOSITED a-SiHx
Year: 1981
Type: article
Abstract: Ion beam deposition (IBD) has been used to prepare a-SiHx thin films over a range of deposition conditions. Concentration of hydrogen in the ion beam is found to be a major factor in determining the properties of these materials. Increasing the hydrogen concentration of the ion beam from 0 to 75% produces a monotonic decrease in room temperature dark conductivity from 10-3 to 10-10 (Ωcm)-1. This is accompanied by an increase in the optical band gap from 1.2 to 1.8 eV and a decrease in the esr spin density to < 1017cm-3. Monohydride SiH bonding predominates in the ir spectra with no evidence for polysilane coordination. Densities are greater than 2.2 g/cm3 for all films made in this study suggesting an absence of voids. Phase contrast TEM gives no indication of columnar morphology.
Source: Le Journal de Physique Colloques
Authors: G. P. Ceasar, K. Okumura, S. F. Grimshaw
Institution: Xerox (United States)
Language: French
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W1990751375