Work

Hydraulic Cement Preparation From Lurgi Spent Shale

Year: 2013
Type: conference-paper
Abstract: Low cost material is needed for grouting abandoned retorts. Experimental work has shown that a hydraulic cement can be produced from Lurgi spent shale by mixing it in a 1:1 weight ratio with limestone and heating one hour at 1000°C. With 5% added gypsum, strengths up to 25.8 MPa are obtained. This cement could make an economical addition up to about 10% to spent shale grout mixes, or be used in ordinary cement applications.
Language: English
Open Access status: green
OpenAlex ID: W201469016
FWCI:
Cites: 1
Cited by: 1
Related to: 10