Work

Catalytic Properties of Gold-zeolites and Related Materials

Year: 2007
Type: dissertation
Abstract: Zeolite catalysts were prepared by carrying out an ion-exchange process of \ntransition metals and impregnation to incipient-wetness method of metal catalyst \nusing a chlorine free gold precursor, KAu(CN)2. The instability of Au/Y \n(3.74wt%Au) resulted in low CO oxidation activity (~ 18 % conversion at 450 \n0C), suggesting that the reduced gold metal atoms are bound to the zeolite by a \nweak interaction. This is subject to migration within the passages of the zeolite \nduring use. The presence of proton stabilized most of Au clusters (electron \ndeficient species) within the HY zeolite, resulting in small amounts of gold \nspecies migrating to the outer surface. Interestingly the CO oxidation activity of \nAu/HY is half that of Au/Y, which clearly indicate that the presence of metallic \ngold plays a significant role during CO oxidation. \nThe loading of Au/M-Y (M = Ni2+, Fe3+, Co2+ or Cr3+) were varied from 1.67- \n7.48wt%Au and from 1.76-5.45wt%M. Modification of this Y structure with \ntransition metals has been found to be beneficial for both activity and stability of \nsmaller gold clusters, by strengthening the interaction between gold and zeolite \nexchange sites and by large magnitude in maintaining the dispersion of gold. This \nsuggests that the unreduced chromium ions function as a chemical anchors for \nreduced Au metal and that the reduced atoms of gold may form small clusters \nwith the anchoring metal. TPR profile has confirmed that the introduction of \n1.67wt%Au on Fe-Y (1.88wt%Fe) increased the stability of Fe ions as stabilizer \nmetal. However, as the gold loading of Au/Fe-Y catalyst increases the TPR profile \nshows that the stability of Fe ions decreases and hence the activity of catalysts. An \nincrease in transition metal content, above 1.88wt%Fe was found to lower the CO \noxidation activity. A TPR profile has confirmed that as the reduction potential \nbecame more negative, the activity of supported Au increases following the \nsequence: Ni2+, 0.23 << Fe3+, -0.41 < Cr3+, -0.56. The estimated particle sizes of \ngold by X-ray diffraction were found to be ~ 12 nm for Ni2+, ~ 7 nm for Fe3+, and \n~ 5 nm for Cr3+ stabilized metal. \nSamples of Au/HY (3.77wt%Au) have been prepared by an ion-exchange method \nusing Au(III) ethylenediamine complex-ions, [Au(en)2]3+. Following a pretreatment \nin an O2 atmosphere, the catalyst showed the existence of an induction \nperiod before reaching a steady state activity; suggesting the need for activating \ngold prior to catalyzing CO oxidation reaction. As-prepared catalyst contained \n85% of gold in the Au3+ valence state as confirmed by Mössbauer spectroscopy. \nThe catalyst was treated with various reducing agents (such as NaBH4); to yield \nstable and active smaller gold clusters (< 2 nm) inside the HY cavities, as revealed \nby X-ray Photoelectron Spectroscopy (XPS), X-ray Diffraction (XRD) and Uv- \nVis Spectrophotometer. DRIFTS revealed that electron-deficient particles (Auó+- \nCO species) of gold clusters, inside the HY framework and in contact with \nprotons are active species for CO oxidation. CO activity and formation of smaller \ngold clusters depends on the nature and molar ratio of reducing agents, and the \nsource of gold. The induction period observed for unreduced Au catalyst is a slow \nstep in the activation of gold active sites. Treatment of Au/Y (3.46wt%Au) with \nsodium borohydride enhanced the activation of gold active species and hence \nimproves the catalytic activity. The NaBH4 treated Au/Y (3.73wt%Au) catalyst \nhas shown, for the first time, activity of approximately 28% CO conversion. The \ncatalyst showed almost the same activity and induction period as that of the \nuntreated Au/HY (3.77wt%Au) catalyst, which leaves much to be investigated \nabout the behaviour of Au on Y zeolite upon treatment with a proper reducing \nagent. The protons have been found to stabilize the smaller Au nanoparticles \nwithin the zeolite cavities. \nThe modification of zeolite-Y was carried out by treatment with different alkali \nmetal nitrates such as LiNO3, NaNO3 and KNO3 before introducing gold from \ndifferent sources, (i.e. gold ethylenediamine complex ion, Au(en)2Cl3; chloroauric \nacid, HAuCl4; or potassium dicyano aurate, KAu(CN)2 complex). The CO \noxidation activity of the catalysts was found to depend on the nature of the gold \nsource and on the type of alkali metal nitrate used. The order of activity was as \nfollows: HAuCl4 >> KAu(CN)2 > Au(en)2Cl3. It was found that the activity of \ncatalysts prepared by deposition of Au from an aqueous solution of chloroauric \nacid on Na-modified zeolites-Y, increased as a result of an increase in the amount \nof Au deposited as confirmed X-ray fluorescence spectroscopy (XRF). The Kmodified \nzeolite-Y had a smaller amount of Au deposited (i.e. Au/KY, \n0.454wt%Au; Au/NaY, 0.772wt%Au and Au/LiY, 0.212wt%Au) and hence the \nCO oxidation activity was lower than that of Na-modified zeolites-Y. Thus, the \norder of the catalytic activity is as follows: Na > K > Li. The XRD studies have \nrevealed that metallic gold particles sizes do not depend on the nature of alkali \nmetal nitrates used to modify the zeolite-Y surface and the zeolite-Y crystallinity \nhas been maintained. \nMonometallic Au/NaY (0.772wt%Au, treated with NaNO3) was found to be \nactive in ethylene hydrogenation with ~5% conversion. Treatment of catalysts \nwith NaBH4 was found to lower the catalytic activity of the catalysts, contrary to \nactivities observed on CO oxidation and these concluded that cationic gold are \nresponsible for the observed activity. The activity was found to depend on the \nsource of Au used, and the order is as follows; HAuCl4 >> KAu(CN)2 > \nAu(en)Cl3. Bimetallic catalysts of Au/M-Y (where Au represent gold from \nKAu(CN)2, and M = Ni2+, Fe3+, or Cr3+) were found to be more active compared \nto monometallic catalysts due to promotional effect of transition metal. The order \nof activity of the bimetallic system at 260 0C was as follows; Ni2+ >> Fe3+ > Cr3+, \nand at 150 0C, was Ni2+ >> Cr3+ > Fe3+, contradicting the order of activity \nobserved on CO oxidation. Formation of carbonaceous deposits on the surface of \nthe catalyst at temperature higher than 260 0C has been confirmed. \nCu modified Au/TiO2 (anatase, 200m2/g) has been prepared by incipient-wetness \nmethod by either introducing the modifier, before or after Au loading. Such \ncatalysts were found to give high and stable activity for the water-gas shift (WGS) \nreaction, when compared to unmodified Au/TiO2 catalysts. It has been suggested \nthat an increase in activity on modified Au/TiO2, is mainly due to the existence of \na synergetic interaction between Cu and Au, since the activity of both Cu/TiO2 \nand Au/TiO2 is lower than that of bimetallic system. The presence of nitrates on Cuc-Au/TiO2 (c Cu precursor is Cu(NO3)2*2.5H2O) has been found to be \ndetrimental to the activity of Au on TiO2; due to the poisoning of Au active sites \nand enhancement of Au agglomeration by NO2 \n- formed during the reaction. An \nincrease in Cu loading lowers the activity of Au. A XANES spectrum has \nconfirmed that gold exists as either Au+/Au0 during WGS reaction and Cu exists \nas copper ions (Cu+/Cu2+) before and during WGS reaction. Formation of \nbimetallic particles was not detected by EXAFS data analysis. The observed \neffects are interpreted as a mutual influence of gold and copper ions and reduced \nspecies of gold and copper due to their competing for ion exchange sites. Cu has \nno promotional effect on low temperature CO oxidation and on preferential CO \noxidation in excess of hydrogen.
Language: English
Open Access status: green
OpenAlex ID: W204509422
Cites: 167
Cited by:
Related to: 10