Abstract: Through oxide phosphorus implantation into silicon substrates with 2.5 × 10 16 /cm 2 at 2–4 keV is investigated as an impurity deposition. Defects and carrier concentration profiles in the substrates are described in the case of drive-in at 1100°C. It is shown that the density of defects is reduced to 10 5 /cm 2 for the doping of 1 × 10 16 /cm 2 phosphorus by optimizing the ion energy and oxide thickness (for example, 3 keV and 130 Å).