Year: 2014
Type: dissertation
Abstract: Heat sealing is the process to achieve the hermetic closure of a package by applying heat and pressure on two polymer films for a specified dwell time. The heat sealing process has been used in packaging of a wide spectrum of products, in particular for food packaging. During the past two decades, heat sealing machinery has been developed for very high speed line production which requires very precise process condition and material optimization. Heat seal process conditions, including temperature, dwell time, and pressure as well as film characteristics such as molecular weight, molecular weight distribution, long and short chain branching are the key factors that control the final quality of the joint. In the first part of this study, we have investigated the interrelated influence of heat seal process parameters on the strengthening of the interface as well as the micro mechanisms involved. The effects of heat seal temperature, pressure, and dwell time on seal strength of LLDPE were illustrated in “time-temperature” and “pressure-temperature” 3D maps, a methodology that is easily applicable to other systems. The interfacial adhesion of semicrystalline polymers was not well understood. We thus studied the adhesion behaviour of LLDPE as a semicrystalline polymer. The results indicated that the time and temperature dependence of seal strength is a consequence of the fraction of amorphous phase available at the interface of films. The seal strength had a linear correlation with the square root of sealing time which was also supported by the welding models. The slope of this linear correlation increased with temperature. This work was followed concurrently by two main approaches: analysis of polymer chain behaviour from microscopic point of view based on reptation theory and conventional macroscopic analysis based on bulk properties of the polymer. Failure mechanisms and fractured surfaces were also analyzed after peeling. Moreover, the topography and morphology of peeled surfaces, which were sealed at different heat seal conditions, were investigated by AFM and SEM. In the debonding failure mode, the crack propagation caused numerous highly oriented fractured craze fibrils on the peeled surfaces. The fractured fibrils were visible in AFM and SEM peeled surfaces of samples sealed at low temperatures. In specimens sealed at higher temperature the fibrillar morphology developed into thicker and larger fibrils. This behaviour was a result of better wetting and interdiffusion by increasing temperature.
Author: Zahra Najarzadeh
Language: English
Subfield: Polymers and Plastics
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2102406870