Formation of NiSi-Silicided p[sup +]n Shallow Junctions Using Implant-Through-Silicide and Low-Temperature Furnace Annealing
Year: 2003
Type: article
Abstract: NiSi-silicided shallow junctions are fabricated using implantation into/through thin NiSi silicide layer (implant-through-silicide technology) followed by low-temperature furnace annealing (from 550 to 800°C). The NiSi film agglomerates following a thermal annealing at 600°C and may result in the formation of discontinuous islands at a higher temperature. The incorporation of fluorine atoms in the NiSi film can retard the formation of film agglomeration and thus improving the film's thermal stability. The forward ideality factor of about 1.02 and the reverse current density of about 1 nA/cm 2 can be attained for the NiSi junctions fabricated by implantation at 35 keV to a dose of followed by a 650°C thermal annealing; the junction formed is about 60 nm measured from the NiSi/Si interface. Activation energy measurement indicates that the reverse bias junction currents are dominated by the diffusion current, indicating that most of the implanted damages can be recovered after annealing at a temperature as low as 650°C. © 2003 The Electrochemical Society. All rights reserved.
DOI: 10.1149/1.1599851
Authors: Chao-Chun Wang, Chiao-Ju Lin, Mao-Chieh Chen
Institution: National Yang Ming Chiao Tung University
Language: English
Field: Materials Science
Domain: Physical Sciences
Open Access status: bronze
Funder: National Science Council
OpenAlex ID: W2125529161