Work

Fluidized bed roasting of micro-pelletized zinc concentrate: Part II- Particle entrainment and residence time

Year: 2011
Type: article
Abstract: Zincor uses O2 enrichment (up to 26% O2 in the fluidizing air) to \nincrease the processing rate of zinc concentrates in the fluidized bed \nroasters. The aim of this study is to determine whether O2 \nenrichment can be reduced by introducing micro-pelletized \nconcentrate into the feed blend, while maintaining current roaster \nfeed rates and calcine quality. It was found that, with a load of 20% \nmicro-pellets introduced into the feed blend, that O2 enrichment \ncould be reduced by 60%. It was determined that entrained particles \nspend on average between 0.46 hour and 2.44 hour in the roaster, \ncompared to particles remaining between 3.93 hour and 4.00 hour in \nthe bed overflow. This compares well with a radioactive tracer test \nperformed by Spira. The required reaction time for micro-pellets was \nfound to be less than the residence time inside a Zincor roaster. The \nresult achieved indicated that the average particle residence time \ninside the roaster was increased successfully in order to compensate \nfor the longer reaction time required to roast micro-pellets at lower \nlevels of O2 in the fluidizing air.
Language: English
Open Access status: green
OpenAlex ID: W2138914087
FWCI: 0.27
Cites: 7
Cited by: 9
Related to: 10