Extraction of Lithium from Lepidolite Using Mixed Grinding with Sodium Sulfide Followed by Water Leaching
Year: 2015
Type: article
Abstract: Mixed grinding with Na2S followed by water leaching was performed to extract Li from lepidolite. The leachability of Li increases dramatically in the ground mixture, regardless of the mixing ratio over the range of 1:1 to 3:1, while only 4.53% of Li was extracted in lepidolite ground without Na2S. The leachability increased with an increase of the grinding time, and ultimately, 93% of the Li was leached by water from the ground mixture with a weight ratio of 3:1 (Na2S:Lepidolite). In the process of the mixed grinding, the Li-contained lepidolite was destructured crystallographically, and it might have changed to different compounds. This process enables us to extract Li from lepidolite via a water leaching treatment.
Source: Minerals
DOI: 10.3390/min5040521
Author: Jaeryeong Lee
Institution: Kangwon National University
Language: English
Subfield: Metals and Alloys
Field: Materials Science
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $2,896
OpenAlex ID: W2180661788