Work

Strength properties change in birch veneered high density fiberboard

Year: 2010
Type: article
Abstract: Strength properties change in birch veneered high density fiberboard. Research consists of modulus of elasticity and static bending strength of high density fiberboard veneered with birch at both sides. urea formaldehyde resin was used for gluing, at 120, 160 i 200 g/m 2 loads at back side of the board, and at 120 g/m 2 on front side of the board. Bending strength and modulus of elasticity were tested with testing machine on both sides. It was concluded that veneering boards with birch increases its mechanical properties, increase of back side glue load from 120 to 200 g/cm 2 increases strength of the composite. 2. Back side at 160g/m 2 , front side at 120g/m 2 glue load. 3. Back side at 200g/m 2 , front side at 120g/m 2 glue load. Packets were pressed in 125 o C, during 5 min. at pressure of 2 MPa. Every board was cut into 150 x 50 mm strength test samples. Each samples group was randomly divided into 10 pieces of back side up and 10 pieces of front side up sets. Strength and modulus of elasticity tests were performed in ten times in both groups, frond side up and back side up. Veneer grain direction was parallel to sample length in each case. The same tests were made
Language: English
Open Access status: diamond
OpenAlex ID: W2183287159
FWCI:
Cites:
Cited by:
Related to: 10