Measurement and control of a residual oxide layer on TiSi/sub 2/ films employed in ohmic contact structures

Year: 1996
Type: article
Abstract: An inadvertent oxide layer is formed on a titanium disilicide (TiSi/sub 2/) film following various wet and dry processes in a manufacturing environment. The use of H/sub 2/SO/sub 4/:H/sub 2/O/sub 2/:H/sub 2/O (1:1:5) as a wet etch for excess Ti metal, prior to the high temperature anneal used to form a subsequent TiSi/sub 2/ layer, is identified as the source of the undesired oxide via multiwavelength spectroscopic ellipsometry and Auger electron spectrometry studies. This inadvertent oxide layer on TiSi/sub 2/ is shown to form bad electrical contacts and is a contributing source to large standby currents in polysilicon gate shunts. Spectroscopic ellipsometry is shown herein as a unique analytical tool to determine both the thickness and structure of this poorly structured oxide during process development. A single wavelength ellipsometer monitoring scheme for both the appearance as well as the thickness of this inadvertent oxide layer is proposed for use in high-volume manufacturing.
Language: English
Open Access status: green
OpenAlex ID: W2069298109
FWCI: 0.252
Cites: 10
Cited by: 4
Related to: 8