Thermo-mechanical properties of glass-ceramic solid oxide fuel cell sealant materials

Year: 2013
Type: dissertation
Abstract: The reliable operation of solid oxide fuel cell stacks depends strongly on the structural integrity of the sealing materials. In this respect, failure and deformation are aspects which need to be assessed in particular for glass ceramic sealant materials. The current study concentrates on the glass ceramics abbreviated H-P (YSZ particle reinforcement) and B. Indentation tests have been carried out to determine elastic modulus, hardness and fracture toughness. Bending tests and compressive tests were carried out at room temperature and typical stack operation temperature for bar and head-to-head jointed glass ceramic sealant specimens, similar as in a stack application with different degree of crystallization and annealed temperature, from which fracture stresses and viscosity values are derived. The results reveal a decrease of the strength for the partially crystallized sealant H-P at operation relevant temperatures that can be associated with the viscous deformation of the material, whereas a stable strength was obtained for the annealed sealant H-P and non-annealed sealant B at operation relevant temperatures that can be associated with the enhanced crystallization of the materials. The experimentally obtained strength data of sealant H-P and B as a function of loading rate are used to assess the effect of subcritical crack growth yielding a failure time under static loading via a strength-probability- time plot that can be used for life time prediction. Fractographic analyses based on a combination of optical, confocal and scanning electron microscopy gives insight into the failure origins.
Authors: Yilin Zhao, Tilmann Beck
Language: English
Open Access status: green
OpenAlex ID: W2201040735
Cites:
Cited by: 12
Related to: 10