Abstract: Acidic sulfates, mainly NaHSO 4 and Na 2 S 2 O 7 , are highly corrosive when molten. Liquid NaHSO 4 is formed as a result of a direct reaction between Na 2 SO 4 in the deposit, and SO 3 and H 2 O in the flue gas. Once formed, it decomposes rapidly into solid Na 2 S 2 O 7 and H 2 O. Solid Na 2 S 2 O 7 , which is noncorrosive, may revert to the corrosive liquid NaHSO 4 if the H 2 O content in the flue gas exceeds a critical value.This critical H 2 O content increases with temperature, which is consistent with the regression relationship log P (atm) = 3.598 – 2.300 x 10 3 /T suggested by Ingraham and Hotz.The re-formed liquid NaHSO 4 causes tube wastage if the deposits at the tube surface do not contain sufficient Na 2 CO 3 to neutralize it.The risks of acidic sulfate corrosion are higher for low-pressure boilers, particularly boilers that are operated at low bed temperatures, with low solids firing, high sulfur input, and high sootblowing steam consumption.
Source: TSpace (University of Toronto)
Authors: Honghi Tran, Nurez Mapara, David Barham
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2246590657