Abstract: Premature failure of Low Temperature Co-Conversion Catalyst in industrial converters IS mostly due to poisoning by sulphur and chlorine.The present study was undertaken with four varieties of commercial catalysts to determine the quantitative relationship between the amount of poison and the extent of deactivation.The results show that poisoning is cumulative in nature and the loss of catalyst activity depends on the total amount of poison as well as its rate of introduction.The poisoning curves generally indicate homogeneous absorption of the poison.Some amount of pore mouth poisoning also takes place.The activity of the fresh and the poisoned catalyst bears a linear relationship with copper surface area of catalyst.The higher the loss of copper area, the more severe is the deactivation.Again loss of copper area does not depend on the copper content or copper surface area of fresh catalyst.Alumina containing catalyst seems to have high sulphur tolerance.
Language: English
Open Access status: green
OpenAlex ID: W224784644
FWCI:
Cites: 3
Cited by: 4
Related to: 8