Direct Determination of Solid-Electrolyte Interphase Thickness and Composition as a Function of State of Charge on a Silicon Anode
Year: 2015
Type: article
Abstract: With the use of neutron reflectometry, we have determined the thickness and chemistry of the solid-electrolyte interphase (SEI) layer grown on a silicon anode as a function of state of charge and during cycling. We show the chemistry of this SEI layer becomes more LiF like with increasing lithiation and more Li–C–O–F like with delithiation. More importantly, the SEI layer thickness appears to increase (about 250 Å) as the electrode becomes less lithiated and thins to 180 Å with increasing Li content (Li 3.7 Si). We attribute this “breathing” to the continual consumption of electrolyte with cycling.
Institutions: Oak Ridge National Laboratory, Los Alamos National Laboratory
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2258786606