Structure of a Spark Plasma Sintering Synthesized (Bi,Sb)2Te3 Based Bulk Thermoelectric Material
Year: 2015
Type: article
Abstract: Bulk nanostructured BixSb1−xTe3 based material was fabricated with spark plasma sintering (SPS) method. The starting powders with a particle size of 10—12 nm were prepared by ball milling. The regularity of fine structure changes as a function of sintering temperature in the 250—550 °C range was investigated by X−ray diffractometry, scanning and transmission electron microscopy (TEM, HRTEM). For the first time coherent dispersion areas (CDA) size was found not to increase monotonously with sintering temperature, and at temperatures of above 400 °C the CDA size decreased as a result of repeated recrystallization. Apparently, the structural changes are associated with a redistribution of intrinsic vacancy type structural defects during sintering.
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: hybrid
OpenAlex ID: W2292662786