Ag/ZnO and Ag/SnO2 Electrocontact Materials Obtained from Fine-Grained Coprecipitated Powder Mixture
Year: 2012
Type: article
Abstract: The manufacturing processes of Ag/ZnO and Ag/SnO2 electrocontact materials concerns to chemical precipitation of precursors are represented in this paper. At all stages, obtained powders and compacts were characterized by X-ray fluorescence (XRF), X-ray diffraction (XRD), thermal analysis (TG, DSC, DMA) and scanning electron microscopy (SEM). The size of particles in the sintered molded article is in the range of 0,1-0,3 nm for ZnO and 1-5 μm for SnO2. The particles size mostly depends on chemical precipitating conditions and metallurgical stage parameters. Relative density of final compacts is about 0,97-0,99. Resistivity is 2,5 cm for the concentration of ZnO equal 8 % and 2.4 cm for the concentration of SnO2 equal 10 %. Electrical wear (AC, test device, 380 V, 30 А, cos =0,8) depends on oxide content and exceeds Ag/CdO series contacts wear.
Institution: Siberian Federal University
Language: Russian
Subfield: Mechanical Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2188321448