Abstract: Se- and S-doped a-Si:H films were prepared by the decomposition of H 2 Se and H 2 S with SiH 4 gas mixtures by plasma enhanced chemical vapour deposition (PECVD) in a ratio of H 2 Se/SiH 4 =1.0×10 - 4 to 1.0×10 - 1 and H 2 S/SiH 4 =6.8×10 - 7 to 1.0×10 - 4 . The dielectric constant of Se- and S-doped a-Si:H films vary with doping concentration and can be tailored by changing the gas ratio. The dc dark and photoconductivity showed a maximum at H 2 Se/SiH 4 = 10 - 3 and a-Si,S:H at H 2 S/SiH 4 = 1.0×10 - 4 and the activation energy is lower at these doping levels. The room temperature dark and photoconductivity in Se and S-doped a-S:H films have been found to increase as the gas ratios increase for H 2 Se/SiH 4 = 10 - 3 and H 2 S/SiH 4 = 10 - 4 , after this range in Se-doped, the dark and photoconductivity decrease to the alloy range.
Authors: Sanjeev Sharma, J. Baveja, R.M. Mehra
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W2472267291