Work

Characterizations of CuInGaSe(CIGS) mixed-source and the thin film

Year: 2010
Type: article
Abstract: CuInGaSe(CIGS) mixed-source was prepared by hydride vapor phase epitaxy (HVPE). Each metal was mixed in regular ratio and soaked at $1090^{\circ}C$ for 90 minutes in nitrogen atmosphere. After making the mixed-source to powder state, the pellet was made by the powder. The diameter of pellet is 10 mm. The CIGS thin film was deposited on soda lime glass evaporated Mo layer bye-beam evaporator. To confirm the crystallization, we measured X-ray diffraction (XRD). High intensity X-ray peaks diffracted from (112), (204)/(220), (116)/(312) and (400) of CIGS thin film and from (110) of Mo were confirmed by XRD measurement.
Language: Korean
Open Access status: bronze
OpenAlex ID: W2028901362
FWCI:
Cites: 15
Cited by:
Related to: 9