Effect of sintering time on particle size of rare earth compounds (R = Nd) prepared by wet chemical method
Year: 2009
Type: article
Abstract: Microstructure of nanocrystalline Nd 2 O 3 supported on amorphous SiO 2 upon heat treatment in air at 700°C for 8-32 h has been studied by means of X-ray diffraction (XRD), Fourier transformation infrared (FTIR) and scanning electron microscopy (SEM). It has been found that the annealing time and sintering temperature played a pivotal role to obtain hexagonal and cubic neodymium oxide. The sample calcined at constant sintering temperature 700°C for 32 h was cubic Nd 2 O 3 nanocrystallites with average size ~10 nm.
Author: Surender Duhan
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W2518199897