Work

Einflussfaktoren auf das Sprödbruchverhalten im Fallgewichtsversuch

Year: 2014
Type: dissertation
Abstract: The drop weight test according to the Battelle Memorial Institute (Battelle Drop Weight Tear Test) is a standardized basis for the evaluation of crack arrest ability of linepipe steels. Similar to the Charpy V-Notch test a pre-notched specimen will be broken with a weighted fin. The ability for crack arrest is subsequently measured indirectly via the shear area percentage of the fracture surface. In contrast to the Charpy V-Notch test, the enlarged dimensions of the test in combination with the high toughness of modern linepipe steels, is pressing the test method more and more to the limits of applicability. The fracture surface shows brittle areas in the by the hammer work-hardened field, which can not occur at the prescribed stable crack propagation (inverse fracture). Even the appearance of a fracture surface consistent with the standard raises doubts: Thus, the brittle splits (separations) parallel to the rolling plane favor the shear area percentage, but reduce the energy. In order to guarantee the safety of gas pipelines anymore, the processes in the drop weight test must be examined carefully. Each component in specimen fabrication and testing, starting from the notch insertion up to the drop weight volocity, contributes to the finally evaluated shear area percentage. The performed experiments show that the brittle initiation, the separations and the inverse fracture are dependent in particular on the specimen thickness, the notch geometry and the impact energy. With increasing specimen thickness the transition temperature rises on the one hand, and on the other hand, the number of separations rises, too. The frequently requested alternative notch shapes to avoid the inverse fracture do not seem to be effective. The probability of a brittle initiation increases with sharper notches, but even after brittle crack initiation the inverse fracture can not be avoided. The rise in the impact energy leads to an enlarged brittle surface in the area of the hammer impact. Based on a large data set, which enables with 57 transition curves in combination with two EBSD measurements in each case a robust modeling, the finding is derived, that the shear area percentage can be increased through targeted adjustment of the microstructure. Lath-shaped structures of high dislocation density as upper or lower bainite have a negative effect on the test results. In addition, the grain boundaries should exceed a certain misorientation (high angle grain boundaries) so that the transgranular crack propagation is impeded. Also, an influence of texture was found. The position of the main cleavage fracture plane {100} determines the characteristics of separations and inverse fracture. While the texture component {100}<011> has often been associated with the separations, the size of the inverse fracture could be connected to the intensity of the {211}<01-1> component for the first time. The investigations show that the BDWT test, which has become a central issue in the development of high-toughness line pipe steels, is influenced by testing, microstructure and texture. On the one hand, the test methodology needs a revision of the standard to minimize the influence of testing conditions and, on the other hand, the individual brittle areas can be reduced by the generation of a specific microstructure.
Authors: Sebastian Scholl, Wolfgang Bleck
Language: German
Open Access status: green
OpenAlex ID: W2591980478
Cites:
Cited by: 1
Related to: 10