Energy Dispersive Spectroscopy Characterization of Solute Segregation in Ti-6Al-4V
Year: 2011
Type: article
Abstract: Ti-6Al-4V, or Ti-6-4, remains the most widely used titanium alloy in the US market.There remains little or no work investigating the Energy Dispersive Spectroscopy (EDS) characterization of solute segregation in Ti-6-4 as a function of sample geometry.Specifically, there are limited investigations of reduced sample thickness and its effects on measured sample composition.Using a vertically oriented drop furnace, samples of α/β processed, mill anneal Ti-6-4 were held at temperatures of 954°, 899°C, 843°C, and 788°C followed by a water quench.The resulting microstructures contained primary equiaxed alpha (α) and martensitic, prior-β regions.EDS characterization of heat treated samples was conducted for bulk samples in the SEM, electropolished thin foil samples in the TEM, and samples thinned to 250-350nm in the focused ion beam (FIB) that were investigated at 12.5, 15, and 20 keV.Vanadium was the solute of interest for this analysis since it exhibits pronounced segregation between the primary α and prior-β regions, as illustrated by the pseudo-binary β isomorphous phase diagram for Ti-6-4.Generally, bulk SEM and thin foil TEM EDS analyses for vanadium concentration were in good agreement with one another.However, a trend of decreasing aluminum concentration with increasing accelerating voltage was observed in the thinned SEM samples.Conversely, measured vanadium concentration increased with higher iii accelerating voltages.For the 954°C heat treatment, vanadium concentrations ranged from 0.3 to 0.9 wt.% for the α phase and from 2.7 to 3.1 wt.% in the prior-β regions.The 899°C heat treatment resulted in vanadium concentration ranges from 0.7 to 1.0 wt.% in the α and 4.3 to 4.5 wt.% in the prior-β region.The measured vanadium concentration for the 843°C heat treatment was between 0.7 to 1.3 wt.% for the α phase and from 4.9 to 5.3 wt.% in the prior-β.The 788°C heat treatment resulted in vanadium concentrations of 1.5 to 1.9 wt.% in the α and 8.6 to 9.6 wt.% in the prior-β region.iv Dedicated to family and friends for their continued support.v Acknowledgments I would like to thank Professors Hamish Fraser and Jim Williams for their support and guidance during my work.Through their support, I have been able to utilize state of the art materials characterization equipment available in the Campus Electron Optics Facility.I would also like to thank everyone in the Fraser Research Group for their collaborative advice and friendship.It has been a pleasure to work with such highly talented individuals.
Author: Brian M. Peterson
Institution: The Ohio State University
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2595673004