Year: 2010
Type: conference-paper
Abstract: Although several working conditions are known to be damaging to Proton Exchange Membrane Fuel cells (PEMFC), their degradation mechanisms are not fully understood yet [1].For instance, supplying the fuel cell with dry gases can induce a fast degradation of the electrodes [2] but on the other hand, long-time or repeated storage without purging liquid water from the gas channels accelerates the fuel cell aging.Potential cycling [3] or operation under open-circuit conditions [4] are also to be avoided.This paper reports about an experimental and numerical study of the internal currents that occur during fuel cell start-up under open-circuit conditions.Shut-down/start-up cycling results in performance degradation according to Tang et al.,.During start-up, hydrogen pushes oxygen, air, or possibly nitrogen that was introduced for purging water toward the outlet so that for a short time depending on various parameters like the flow rate and the channels geometry, a fraction of the anode compartment is filled with hydrogen while the other part is still occupied by the gas initially present.A potential appears at the inlet of the anode but not at the outlet, which generates internal currents under open-circuit conditions.Although these internal currents are scarcely studied, they were modelled by some authors [8-10] and they can be measured using segmented cells [11,12].According to Meyer and Darling [9] internal currents can be at the origin of fuel cell performance decay by creating abnormally high potentials at the cathode, causing carbon corrosion.Starting from experimental data measured thanks to a segmented cell, Siroma et al. [11] suggested that the double layer capacitance could play a major role in the origin of reverse currents and high potentials.
Source: JuSER (Forschungszentrum Jülich)
Language: German
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W2604475809