The impact of brannerite on the release of plutonium and gadolinium during the corrosion of zirconolite-rich titanate ceramics
Year: 2000
Type: article
Abstract: Titanate ceramics have been selected as the preferred waste form for the immobilization of excess plutonium. Corrosion tests are underway to try to understand the long-term behavior of this material. In this paper, results from PCT-B static dissolution tests are used to provide an explanation of the observed corrosion behavior of a zirconolite-based ceramic. Two important observations are made. First, Ca is released at a constant rate [7 x 10{sup {minus}5} g/(m{sup 2} day)] in PCT-B tests for up to two years. Second, the release rates for Pu and Gd increase with time (up to two years) in PCT-B tests. The first observation suggests that the ceramics continue to corrode at a low rate for at least two years in PCT-B tests. The second observation suggests that the release rates of Pu and Gd are controlled by some process or processes that do not affect the release rate of other elements. Evidence indicates that this is due to the preferential dissolution of brannerite from the ceramic.
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
Funder: U.S. Department of Energy
OpenAlex ID: W268091124