Work

Influence of Cr2O3 additive and sintering temperature on the structural characteristics and piezoelectric properties of Bi4Ti2.95W0.05O12.05 Aurivillius ceramics

Year: 2016
Type: article
Abstract: In this paper, Cr 2 O 3 (0–0.4 wt%) as an additive was added into Bi 4 Ti 2.95 W 0.05 O 12.05 (BITW) for preparing a kind of W/Cr co-doped BIT (BITW-yCr) Aurivillius ceramics, both W 6+ and Cr 3+ are considered to substitute Ti 4+ in the [TiO 6 ] octahedron of BIT. Besides the orthorhombic Bi 4 Ti 3 O 12 as the major phase, BITW-yCr ceramics also contain the cubic Bi 2 Ti 2 O 7 as the second phase which was formed due to the doping effect of WO 3 , but its formation could be depressed by the addition of less Cr 2 O 3 . Additionally, the cell parameters of BITW ceramics are also changed by the incorporation of Cr 2 O 3 , as the distortion degree of the orthorhombic structure ( a / b ) increases firstly and then decreases with its addtional amount (y). On the other hand, the grain growth of BITW-yCr ceramics is mainly controlled by the sintering process, there a higher sintering temperature results in a larger grain size. In comparison to BIT ceramics, BITW-yCr ceramics with less Cr-addition (y=0–0.2) require a higher sintering temperature to attain the best dense state, moreover, as y increases, the sintering temperature to gain the highest piezoelectric activity also increases. Finally, BITW-0.2Cr which was sintered at 1150 °C exhibits a higher piezoelectric activity than the others, which could be attributed to its larger orthorhombic distortion and larger grain size, its ideal piezoelectric constant ( d 33 =28 pC/N) provides it with great applying potentiality.
Language: English
Open Access status: hybrid
Estimated APC paid: $2,790
OpenAlex ID: W2565092839
FWCI: 0.3
Cites: 30
Cited by: 15
Related to: 10