Hot Corrosion of Advanced Nickel-Based Disk Alloys

Year: 2013
Type: article
Abstract: The objective of this work was to evaluate and compare Type I and Type II hot corrosion in two different nickel-based disk alloys (Rene 88 and Rene 104) when exposed to a mixed salt in the temperature range of 704 -788°C (1300 -1450°F).Testing was conducted from exposure times of 10 min to 24 h.For results indicating Type II attack, pit initiation, morphology, growth mechanisms, pit growth rates were compared using scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and optical profilometry (OP).Type I attack was evaluated using only SEM and EDS.Testing at 704°C revealed that a Type I attack was prevalent, with localized attack in the form of pitting initiating at exposure times as short as 10 min.Pit initiation occurred on tantalum-rich carbides for Rene 104.Pitting initiated on Rene 88 by an undetermined method.After initiation, the pit morphology was similar in both alloys; nickel oxide and cobalt oxide deposits on the surface, chromium oxide compromising the majority of corrosion product inside the pit, and a layer of sulfide between the pit and base alloy.The pit growth rates were likewise determined to be very similar across alloys, proving that control of Type II hot corrosion resides in preventing pit initiation.Higher temperature testing at 760 o C displayed mixed results.Alloys Rene 88 and Rene 104 initiated Type II attack after 15 min exposure.Pits grew to approximately 10 µm in diameter at 0.5 h.At this point, pit growth ceased and a broad Type I attack iii initiated, with chromium sulfides present beneath the surface of the alloy.The highest temperature tested, 788 o C, yielded similar results across all both alloys.Both alloys display Type I hot corrosion with a depth of attack reaching a maximum of 3 -5 µm.No Type II hot corrosion was detected at this temperature.When compared to other temperatures, the Type II attack observed at 704 o C, was the most severe attack observed.While the Type I attack covered more surface area, the Type II pitting attack observed reached a depth of attack on the order of 100 µm.
Author: John F. Guzowski
Language: English
Open Access status: green
OpenAlex ID: W2903293636
FWCI: 0.158
Cites: 22
Cited by: 1
Related to: 10