Work

Development of more sustainable polymers and composites materials based on 2,5-furandicarboxylic acid

Year: 2019
Type: dissertation
Abstract: Nowadays environmental problems, climate changes, limited fossil resources and their price fluctuation, associated with industrial activity (often ecologically unsound) are the strong driving forces for governments, companies and scientists to find alternatives to the fossil-based materials. In this scenario 2,5- furandicarboxylic acid (FDCA), a renewable platform chemical has emerged as the most promising substitute to terephtalic acid for the synthesis of several materials, particularly polyesters, which possess similar thermal and mechanical proprieties. These materials could be applied to current applications and, could even be applied in new, innovative and high value applications. In this context, the development of sustainable FDCA-based polymers and materials is timely and quite relevant. Precisely, the main objective of this thesis is the development of more sustainable polymers and composites based on FDCA and a wide panoply of aliphatic compounds selected for their renewable origin (PART B) and/or the improved thermal and mechanical properties they can impart the ensuing materials. Furthermore, the potential of a new FDCA-based ester monomer as plasticiser for partial replacement of the non-renewable di(2- ethylhexyl) terephthalate on PVC formulations was also evaluated (PART C). In the first study, a partially renewable polyester based on FDCA and 1,4- cyclohexanediol, namely poly(1,4-cyclohexylene 2,5-furandicarboxylate) (PCdF) was prepared aiming at preparing a new material with enhanced thermal properties. Its synthesis was performed by two distinct approaches, namely via solution polycondensation and bulk polytransesterification. For comparative purposes, poly(1,4-cyclohexanedimethylene 2,5-furandicarboxylate) (PCF) homopolyester was also synthesised, due to their related structural resemblance. Homopolyesters with different molecular weights (Mn and Ð values ranging between 4 300-14 100 g/mol and 1.2-1.7, respectively) were obtained, depending on the synthesis approach and catalyst used. The resulting materials revealed to possess semi-crystalline character with high glass transition temperatures (Tg values of 175 and 105 ºC for PCdF and PCF, respectively), and thermal stablility up to 377 ºC. It was also found that, the absence of the methylene group on PCdF homopolyester, lead to a more rigid polymer chain backbone, and accordingly to a highest Tg. Other studies, focused on the development of copolyesters enterelly based on renewable-based monomers, namely those based on FDCA, 1,4-butanediol and poly(propylene oxide) or diglycolic acid were performed. In a second study, several poly(1,4-butylene 2,5-furandicarboxylate)-copoly( poly(propylene oxide) 2,5-furandicarboxylate) (PBF-co-PPOF) poly(esterether) s copolymers were synthesised using dimethyl 2,5-furandicarboxylate and different molar ratios of 1,4-butanediol and poly(propylene oxide). The ensuing copolyesters presented either semi-crystalline character when using higher PBF feed amounts, or completely amorphous viscous liquid was obtained instead when using a PBF/PPOF ratio equal to 1 . Moreover, these materials presented high thermal stability (maximum degradation temperatures between 340-365 ºC), and low Tgs (values ranging from -42.3 to -32.6 ºC), facilitating their processability at lower temperatures. Further, in a third stud, comprised the preparation of a series of FDCA-based nanocomposites were prepared using poly(1,4-butylene 2,5-furandicarboxylate)- co-poly(1,4-butylene diglycolate) (PBF-co-PBDG) copolyesters and acetylated bacterial cellulose (Ac-BC). In a first step, PBF-co-PBDG (co)polyesters were synthesised; followed, in a second step, by the preparation of nanocomposites films obtained by solvent-casting approach. Interestingly, for higher incorporation of BDG moieties, these reinforced materials showed an increased stiffness (Young’s modulus up to 1239 MPa) and reasonable elasticity (elongation at break values between 0.6 to 25.0 %) compared to their neat (co)polyester counterparts. Furthermore, similar values of oxygen permeability of nanocomposites and (co)polyesters were observed, expanding the exploitation of these materials for packaging applications. Finnaly, a fourth study, addressed the possibility of using a furanic ester as an additive for poly(vinyl chloride) (PVC). A combination of di(2-ethylhexyl) 2,5- furandicarboxylate (DEHF) and di(2-ethylhexyl) terephthalate (DEHT) plasticisers was performed into an attempt to increase the ‘green content’ of PVC formulations. These materials have shown to possess higher compatibility with the PVC matrix compared with DEHF as single plasticizer, confirmed by FTIR spectroscopy. Furthermore, they displayed thermal features comparable to those prepared with DEHT as single plasticizer (Tg’s between 19.2 to 23.8 ºC), and increased elongation at break (up to 330%). Moreover, migration tests revealed very low weight loss percentages, not exceeding ca. 0.3 and 0.2%, for water and PBS solution, respectively. More important, preliminary results of in vitro cell viability tests (concentrations up to 500 μM for a maximum of 72 h) revealed a non-toxic profile (around 100 %) for both DEHF and DEHT plasticisers. All FDCA-based materials and chemicals prepared under the scope of this dissertation are an important contribute for the increasing demand for new renewable-based products, within a sustainable approach. Further, these materials and chemicals, presented similar or improved properties to those prepared from petroleum-based resources.
Author: Marina Matos
Language: English
Subfield: Biomaterials
Open Access status: green
OpenAlex ID: W2965605397
Cites:
Cited by:
Related to: 10