Composition of Products of Birch Wood Delignification by Hydrogen Peroxide in the Medium oeAcetic Acid $ Water $ Catalyst TiO2B

Year: 2015
Type: article
Abstract: The composition and structure of the solid and soluble products of birch wood delignification by H 2 O 2 in the presence of TiO 2 catalyst were studied.The efficient delignification of wood proceeds at 100 °C and atmospheric pressure.The obtained microcrystalline cellulose (yield 48.2% mass.), has crystallinity index 0.81 and contain 93.7% mass.cellulose, 5.5% mass.hemicelluloses and 0.5% mass.lignin.Soluble products of birch wood peroxide delignification are mainly presented by 4-O-methylglucuronoxylan (84% rel.), monosaccharides and they contain very few aromatic compounds.