Oberflächenmodifikation der Magnesiumlegierung WE43 durch Zink- und Aluminiumbeschichtung und thermische Behandlung
Year: 2014
Type: dissertation
Abstract: With rising interest in a many-sided use of magnesium alloys also the improvement of their corrosion properties become more important. One approach is an aluminium-zinc-coating with following thermal treatment. Therefore, central of this work is the thermal treatment of aluminium- and zinc-coated samples of the magnesium alloy WE43. Furthermore, the applicability of this coating-system on a stent is tested. In the arranged experiments electrochemically aluminium- and zinc-coated WE43- and puremagnesium-flatsamples, as well as WE43-stents were heat-treated in argon. The in this way resulting surface modifications are determinated by the formation of the binary Al-Mg-phases Al3Mg2, Al30Mg23, Mg17Al12 and the ternary tau-phase (Al,Zn)49Mg32. At very short heat treatments there are also observed Mg-Zn-phases. The tau-phase exists in its full homogeneity range. Rich in zinc at short and poor in zinc at intensive heat treatments. Additional to the tau-phase there are binary Al-Mg-phases at intensive thermal treatments. The magnesium-richer phase Mg17Al12 forms at the interface to the bulk material, the aluminium-richer phases Al3Mg2 and Al30Mg23 form in the near-surface area. Differences in the phase formation between substrate materials exist especially at extreme and short heat treatments. For the examination of the aptitude of the resulting surface modifications for stent application corrosion and dilatation experiments are performed. The corrosion experiments show that an aluminium-zinc-coating leads to an obvious improvement of corrosion-resistance. It is possible to reach a further improvement by a short heat treatment like at 290°C for 5 min. Less satisfying are the results of the testing of the mechanical capacity. None of the surface modified stents, neither the only coated, not heat-treated withstand a dilatation by balloon catheter. Finally, the resulting surface modifications are not suitable for stent application. But the use for other applications requiring non-corrosive magnesium, but not such high ductility, is already possible yet.
Author: Kerstin D. Tillmann
Institution: Friedrich-Alexander-Universität Erlangen-Nürnberg
Language: German
Subfield: Biomaterials
Field: Materials Science
Domain: Physical Sciences
Open Access status: green
OpenAlex ID: W3000431243