Threadline Modification of Poly(ethylene terephthalate) (PET) High-Speed Melt Spinning by Integration of Horizontal Liquid Isothermal Bath (HIB) and Drawing Process.

Year: 2020
Type: article
Abstract: Threadline Modification of Poly(ethylene terephthalate) (PET) High-Speed Melt Spinning by Integration of Horizontal Liquid Isothermal Bath (HIB) and Drawing Process.(Under the direction of Dr. Richard Kotek).Poly (ethylene terephthalate) (PET) is an indispensable and important commercial polymer after being introduced into the consumer market in 1951.More than half of the global PET is used to manufacture PET filaments.Because PET filament has high potential to obtain superior properties such as good resistance, high strength, good resistance to abrasion and good chemical/thermal/dimensional stability, it is utilized in challenging areas such as automotive and aerospace.Therefore, several studies on developing and modifying filament manufacturing processes have been performed in the past few decades by scientists and researchers, such as incremental draw process, quench air flow modification, zone-drawing, and zone annealing.A simple and ecological threadline modification technology during melt spinning named horizontal isothermal bath (HIB) was proposed in Dr.Richard Kotek's Group to manufacture high-performance fiber-forming polymer fibers in 2000.The first HIB model separated the spinning and drawing processes, called two-step HIB processes, and then, in 2019, HIB model was upgraded to the continuous one-step HIB process by integrating spinning and drawing processes.Surprisingly, the HIB technique increased the strength of low molecular weight polymer fibers, even surpassing that of high molecular weight polymer at the same conditions.Low molecular weight Nylon 6 fibers achieved 10.02 g/den in tenacity, and low molecular weight PET fiber achieved 10.23 g/den in tenacity in the past studies.In this study, both low (0.58 g/dL) and high (1.05 g/dL) molecular weight PET polymers were utilized in one-step HIB technique.Besides traditional structure-property analysis, the statistical design of experiment and modeling were also employed to investigate effects of continuous isothermal bath process and optimal strength of corresponding PET fibers in this study.The water was applied as bath liquid across all the experiments because of environmental protection and drawing frame temperatures are fixed.Moreover, in order to increase spinnabilities of PET fibers within one-step HIB process, several modifications of mechanics in the spine line were made in this study.An investigation of structure-property relationship by various characterization techniques for effects of liquid depth, liquid temperature, take-up speed, and drawing ratio is done in the discussion section.The modified split-plot design was employed to randomize sequences of sample spinning before spinning and mixed model for one-step HIB process was built after collecting all the data to quantify effect.At the spinning conditions of 90°C in liquid temperature, 20 cm in liquid depth and 3,600 m/min in take-up speed with draw ratio of 1.20, the high molecular weight PET filament achieved 7.03 g/ den in tenacity and 110.12 g/d in modulus with 10.60% in elongation at break while low molecular weight PET filament achieved 7.21 g/d in tenacity and 127.79 g/den in modulus with 9.69% in elongation at break.At the sample spinning conditions, commercial (control) high molecular weight PET filament has tenacity of 6.93 g/d and modulus of 109.22 g/d with 12.13% in elongation at break at draw ratio of 5.20.Commercial samples need a much higher draw ratio than HIB samples, and therefore the isothermal bath is considered to be a drawing process in spinline.The statistical mixed model contains five main effects, four twofactor interactions and two error terms.Draw ratio has positive effect on tenacity of PET filaments.High level of liquid temperature (90°C), liquid depth (20 cm), and take-up speed (3,600 m/min) led better tenacity than low level of those factors (75°C, 15 cm and 2,800 m/min, respectively).However, low molecular weight PET samples had larger tenacity increments than high molecular weight PET samples in one-step HIB process.Liquid temperature had a larger effect on tenacity on low molecular weight PET filament than high molecular weight PET filaments, whereas changes of take-up speed have larger effect of tenacity on high molecular I would like to express my sincere gratitude to my advisor Dr.Richard Kotek for his patience, encouragement, guidance, freedom and continuous support during my long Ph.D. journey.My special thanks go to my statistical advisors Dr. Justin Post and Dr. Jonathan Stallrich for their patience and guidance in my statistical studies.I would like to extend my gratitude to my textile committee members Dr. Xiangwu
Author: Yan Jiang
Language: English
Open Access status: green
OpenAlex ID: W3021267428
FWCI:
Cites: 120
Cited by: 1
Related to: 10