Abstract: In Polymer electrolyte membrane fuel cells (PEMFC) and direct methanol fuel cell (DMFC) systems, the catalyst is supported on a conductive porous support for high stability and activity. The support should have adequate surface area, porosity, electrical conductivity, electrochemical stability, surface functional groups, and the like. The suitable supports for metal nanoparticle should be included (1) high electrical conductivity (2) high catalyst-support interactions (3) large surface area (4) adequate porous structure to maximize the triple phase interface (5) ease of water management to prevent flooding; (6) high corrosion resistance, and (7) easy recovery of the catalyst. Therefore, the choice of a suitable support will have a key impact on determining the catalyst, and hence the behavior, performance, lifetime and cost of the fuel cell. Until now, carbon black (CB) with high surface area and high conductivity have been widely used as fuel cell catalyst supports. However, since CB is vulnerable to durability such as carbon corrosion or oxidation, research is continuing to find materials that are durable materials. Therefore, many nanostructured materials, including carbon nanostructures, metal oxides and conductive polymers have been extensively studied over the last decades to improve the existing performance of catalyst supports for PEMFC/DMFC and to develop new ones. However, the development of supporting materials that possess high durability while reducing the amount of platinum is becoming very important, so it is not enough to develop supporting materials. Fundamental research is needed to secure catalysts with high durability through the design of catalyst supports that can solve the drawbacks. Representatively, strong catalyst-support interaction is able to improve the cell efficiency and charge mobility while reducing metal catalyst losses. In addition, the support can help improve catalyst performance and durability by reducing poisoning of the catalyst, and also affects the catalyst particle size. \n In this dissertation, I present the result of solving the disadvantage by developing a new support material and identifying the relationship between support and catalyst. And also, it proposes a method to ensure durability through simple engineering of surface of support material. \n To address the issues of the conventional carbon supports, chapter 2 presents carbon nano-onion (CNO), a new class of carbon allotrope, as a support for Pt catalysts. CNO had the spherical shape with 3 to 5 nm in diameter consisting of ~5 concentric graphitic layers. Superior durability of catalytic oxygen reduction reaction (ORR) was guaranteed by Pt supported by CNO (Pt/CNO) due to: (1) the islands-by-islands configuration of the Pt/CNO composites (c.f. islands-on-a-particle configuration for Pt/C) to isolate each Pt nanoparticle from its neighbors by the same-size CNO particles and to suppress Ostwald ripening by highly tortuous void structure; (2) the curvature-induced strong interaction between CNO and Pt; and (3) the graphite-like concentric layers guaranteeing corrosion resistivity. \n In chapter 3, an oxygen reduction reaction (ORR) catalyst/support system was designed to have Pt nanoparticles nanoconfined in nano-dimensionally limited space. Holey crumpled reduced graphene oxide plates (hCR-rGO) were used as a carbon support for Pt loading. As expected from Pt-to-Pt distance of Pt-loaded hCR-rGO longer than that of Pt/C (Pt-loaded carbon black as a practical Pt catalyst), the durability of ORR electroactivity along cycles was improved by replacing the widely used carbon black with hCR-rGO. Unexpected morphological changes of Pt were electrochemically induced during repeated ORR processes. Spherical multi-faceted Pt particles were evolved to {110}-dominant dendritic multi-pods. Nano-confinement of a limited number of Pt within a nano-dimensionally limited space was responsible for the morphological changes. The improved durability observed from Pt-loaded hCR-rGO originates from (1) dendritic pod structure of Pt exposing more number of active sites to reactants and (2) highly ORR-active Pt {110} planes dominant on surface. \n Through the results of this dissertation. researchers related to fuel cell and catalyst materials will be able to summarize the results of the study on catalyst supports and hope to be a reference for future research.
Author: Juchan Yang
Language: English
Open Access status: green
OpenAlex ID: W3032674383
Cites: 143
Cited by:
Related to: 10