Work

ЭКСПЕРИМЕНТАЛЬНАЯ ОЦЕНКА КРИСТАЛЛОГРАФИЧЕСКОЙАНИЗОТРОПИИ ТЕРМИЧЕСКОЙ УСТАЛОСТИ МОНОКРИСТАЛЛОВ СПЛАВА НА ОСНОВЕ Ni3Al ДЛЯ ВЫСОКОТЕМПЕРАТУРНЫХ ДЕТАЛЕЙ АГТД

Year: 2011
Type: article
Abstract: Results of an experimental research of thermal fatigue of single crystals of alloy ВКНА-1В (on the basis of intermetallic NijAl) in conditions thermo-cycles 100«850 °С, 100«1050 °С and 100«1100 °С with a controlled stress in a cycle. On the basis of results of tests of cylindrical monocrystals samples with axial crystallographic orientations <001>, <011> and <111> are received it settlement experimental dependences of number of cycles before destruction from scope of thermal stresses in a cycle for everyone investigated crystallographic orientations. It is established, that on baseline N = 103 thermo-cycles with the maximum temperature of a cycle 850 and 1050 °С the greatest resistance of thermal fatigue has axial crystallographic orientation <111>, and at 1100 °С on this baseline monocrystals of all three orientations practically equally oppose to thermal fatigue. On baseline N = 104 thermo-cycles в at the maximum temperature of a cycle 850°С orientation <111> has the greatest resistance, and at temperatures 1050 °С and 1100 °С — orientation <011>.
Language: Russian
Open Access status: green
OpenAlex ID: W3081963106
FWCI:
Cites:
Cited by: 1
Related to: 10