Abstract: The purpose of this thesis was to find out right process parameters for deposition of porous polycrystalline silicon in a vertical LPCVD reactor. The process window for porous polysilicon is narrow and the parameters vary depending on the used reactor. Chemical vapor deposition (CVD) is used for thin film deposition. Different CVD methods produce films with varying properties and quality. Polycrystalline silicon is deposited with CVD and process conditions affect the structure and properties of deposited film. Polysilicon is a versatile material used in for example surface micromachining. The literature review focuses on CVD, reaction kinetics of CVD and different CVD methods. In addition to that, the properties and structure of polysilicon and fabrication of porous polysilicon are discussed. In the experimental part, the effect of process parameters on deposited polysilicon films were studied by changing process temperature, pressure, and gas flows. The films were characterized by measuring thickness, refractive index, and residual stress. The permeability was tested by wet etching of underlying silicon dioxide film in 50% HF solution for 3 minutes. Etch rate of films in HF vapor was also studied. IR microscope was used to study the etching \nresults. \n \nResults showed that increasing process temperature made polysilicon films more permeable and decreased residual stress and refractive index. Deposition rate increased with increased temperature and decreased with decreased pressure. All the films deposited at 590 °C were completely permeable with compressive residual stress. The films deposited at 584 °C with pressure of 450 mTorr were almost permeable and had low tensile stress. Increasing gas flow made the uniformities worse, hence best film was deposited in run 7 at 584 °C, at pressure 450 mTorr with lower gas flows, silane flows 190 and 170 sccm, with average residual stress of 12 ± 15 MPa. How film thickness affects permeability was studied with reference run and experimental run 7 parameters and it was noticed that films with thickness over 200 nm became impermeable. To improve the thickness uniformities, the parameters were optimized. This was done by adjusting gas flow from 190/170 sccm to 185/164 sccm and by decreasing temperature in the lowest temperature zone from 607 °C to 603.7 °C. This improved the Wafer-to-Wafer Uniformity from 3.7 % to 2.1 % and average Within Wafer Uniformity from 5.5 % to 4.7 %.
Source: Aaltodoc (Aalto University)
Author: Tytti Virtanen
Institution: Aalto University
Language: English
Subfield: Materials Chemistry
Field: Materials Science
Domain: Physical Sciences
Keywords: polycrystalline silicon thin films, chemical vapor deposition, process parameter optimization, deposition temperature, deposition pressure, gas flow rate, film thickness uniformity, wafer-to-wafer uniformity, refractive index, residual stress, permeability, silane precursor, surface micromachining, silicon micromachining
Open Access status: green
OpenAlex ID: W3183538407