Abstract: By using silicate inorganic binders and glass waste (colourless or coloured) it is possible to mould technical and artistic elements, which later can be hardened by means of high temperature processing. This procedure is controlled by both the glass transition temperature of binder and of glass waste used as aggregate. To produce new glasses in these cases have been designed a new compound made of liquid binder (sodium silicate) and ground glass as aggregate from common glass bottles (sodium calcium) colored or not colored. "Water glass", catalysed with sodium hydroxide was used as a binder of glass shards from common industrial bottles, classified to a grain size distribution below 2 mm. Chemical analysis shows similarity of silica content between binder and aggregates of recycled glass, establishing as main differences in the percentages of chromophore oxides. In addition dilatometry curves of the two materials show close glass transition temperature values (575 and 598ºC, respectively), fact that facilitates sintering between binder and aggregates. The non-heat-treated samples present good compactness and mechanical resistance values, improved with heat-treatment at 700ºC. The high compactness of heated samples, showing rounded aggregate grains and softening of binder could let a good way for obtaining well-consolidated technical elements, made of recycled glass. From this test, it would be possible to use thermal ranges between 550 and 600°C, as well as shorter exposure times for a proper hardening. These materials constitute a true substitute for expensive processes, such as the preparation of hot glass. These new products improve technical properties and ease of use that are organic polymers (e. g. epoxy or polyester). The products mechanically finished with this technique can be completed through further compaction with heating to temperatures close to 500 ° C.
Source: Anales de Edificación
Language: Spanish
Subfield: Building and Construction
Field: Engineering
Domain: Physical Sciences
Open Access status: diamond
OpenAlex ID: W3123068075