The Study on Thermal Retraction Behavor of the Heated Polyethylene Terephthalate Fibers (1) Temperature Dependence of the Thermal Contractton in Equilibrium
Year: 1964
Type: article
Abstract: The thermal stability of the heated P. E. T. fiber has been discussed from the viewpoint of a fine structure, as reported in the previous paper 1), 2). Dimensional stability of the thermo-plastic fiber is one of the most important properties for practical purpose and so the oriented P. E. T. fiber under various heated conditions was investigated to find out the temperature dependence of the thermal contraction in equilibrium. And in order to estimate a fine structure of fiber from the percentage of contrction, its value was quantified as a function of the degree of crystallization and orientation factor. The results obtained are ss follows:1) The thermal equilibrium contraction curves are exhibeted with a characteristic sigmoid shape, which shows the percentage contraction increases with rising temperature. The temperature distribution curves of the thermal contraction in equilibrium have two peaks. Its maximum point in a low temperature range shifts towards higher temperature with increasing heatset temperature, while it may disappear at higher heated temperature beyond 170°C. And its distribution may become broader with heatset temperature. On the other hand, maximum position in a high temperature range is not affected by heated condition, but its value becomes larger with increased heatset temperature. The former may be due to a frozen strain occured on production production process, and the latter to the binding strain on drawing and afterheating processes.2) Assuming that the thermal retraction of the fiber may becaused by deorient effect due to break-down of either crystallites or secondary bond among the oriented molecular chains in the amorphous region, then the temperature dependence on the thermal retraction in equilibrium may be represented by the following formula:where: S0: percentage contraction, when these bonds do not break down at all. ST: percentage contraction at giving temperature (T°C) k: constant Nb: numbers of thesebonds among the oriented molcular chains in the amorphous region And considering the degree of crystallization (X) and orientation factor (ƒ), equation (1) may be transformed as follows:And, curves obtained from the equation (2) agrees with experimental results. Consequently, intermolecular aggregation state may be estimated from thermal retraction behaviors.3) Relation between the logarithmic of the thermal equilibrium contaction and the reciprocal of the reciprocal of the absolute temperature may be described by “Arrhenius Plot”. It comprises of three staight lines which have two transition temperatures. While the apparent activation energies obtained from slope of the straight lines decrease in a low temeperature range with increasing heatset temperature, their energies increase at a high temperature range.
Source: Sen i Gakkaishi
DOI: 10.2115/fiber.20.215
Authors: Isamu Kuriyama, Toru Kawai
Institution: Tokyo Institute of Technology
Language: English
Subfield: Polymers and Plastics
Field: Materials Science
Domain: Physical Sciences
Open Access status: bronze
OpenAlex ID: W2318496459