Year: 2024
Type: article
Abstract: Al solid-state MAS NMR spectra. In the subsequent steps, the ball milled material was oxidized in an STA system. Already 5 min of ball milling significantly changes the energy pattern of the reaction. Powder X-ray diffraction studies on the oxidized material clearly indicate that a different reaction pathway occurs. Samples ball milled for 180 min even get pyrophoric.
Source: Dalton Transactions
DOI: 10.1039/d4dt02459a
Institution: Saarland University
Language: English
Subfield: Mechanics of Materials
Field: Engineering
Domain: Physical Sciences
Open Access status: hybrid
Awards: G3137249817, G808732564, G8560120387
OpenAlex ID: W4404333530