Abstract: Si heterojunction (SHJ) solar cells have demonstrated record efficiency >27%, approaching the theoretical limit of ≈ 29%, primarily due to best surface/interface defect passivation provided by deposited thin layers of hydrogenated amorphous silicon (a-Si:H). Such excellent surface/interface passivation reduces recombination loss and result in >100 mV improvement of cell open circuit voltage (VOC) to ≈ 750 mV, thus the cell efficiency. However, fielded SHJ modules exhibit loss of VOC and hence efficiency over time in years, presumably due to degradation related to a-Si:H layers. This adversely affects the technology’s market acceptance, and levelized cost of energy (LCOE). It is hypothesized that the origin of a-Si:H degradation is somehow related to the presence of weak Si–Si bonds and hydrogen in a-Si:H films. The objective of this project is to test this hypothesis by directly measuring chemical and structural changes occurring within SHJ component layers and solar cells. This is achieved by developing an innovative in-situ Fourier transform infrared (FTIR) spectrometry apparatus to monitor hydrogen microstructural changes occurring within amorphous silicon and decipher hydrogen evolution kinetics over time when samples are exposed to heat and/or light stress. These in-situ measured hydrogen microstructural changes are correlated to the changes in effective minority carrier lifetime (τeff), implied VOC (iVOC), surface recombination velocity (S), and cell VOC. These mechanistic understandings will provide critical guidance to mitigate the VOC-driven degradation of SHJ solar cell performance. Passivation optimization and degradation analysis of individual SHJ component structures were achieved through systematic deposition of three symmetric structures and the completed SHJ solar cell structure. The three symmetric structures used were intrinsic a-Si:H [(i)a-Si:H] layers in a bilayer structure, intrinsic and p-type doped stacked layers [(i-p)a-Si:H] representing the front heterojunction in the SHJ cell, and intrinsic and n-typed doped stacked layers [(i-n)a-Si:H] representing the back-side back surface field (BSF) in the SHJ cell. State-of-the-art passivation qualities are demonstrated by a champion iVOC of 740 mV for the (i)a-Si:H layers, and the (i-n)a-Si:H symmetric structure. A 725 mV iVOC is observed for the (i-p)a-Si:H symmetric structure. These symmetric passivated SHJ component structures were subsequently subjected to different accelerated lifetime (ALT) stressors to identify which conditions contribute the most to iVOC degradation. Degradation of the thin (10 nm) (i)a-Si:H passivation layers without any additional overlying layers is minimal; complexity of this study arises due to unavoidable surface oxidation of (i)a-Si:H layer during most of the stress application, which is likely irrelevant for a full SHJ cell configuration with overlying protective layers. The iVOC degradation of symmetric structures is found to occur primarily at the (i-p)a-Si:H passivation stack under dark heat stress with associated hydrogen loss from the (p)a-Si:H layer. An activation energy for increase in S (defect creation) of 0.65 eV can be correlated to the activation energy of ≈ 0.4 eV for hydrogen loss from the (i-p)a-Si:H stack. This also suggests the presence of weakly bonded hydrogen in the (p)a-Si:H films, which effuses out of the film stack at such low activation energy. When light and heat stress are applied together, similar hydrogen loss from (i-p)a-Si:H stack is observed, however, does not appreciably degrade iVOC or increase S. This is an important result and departure from direct correlation between hydrogen loss and defect creation. This perhaps indicates additional defect chemistries or annealing that might be occurring in the presence of light requiring further detailed defect measurements. The full SHJ cell structure used for this project is depicted in Fig.1(d). SHJ cells with an initial VOC ≈ 700 mV were fabricated and subjected to similar ALT stress conditions. Cell VOC is found to degrade the most under dark heat stress and is confirmed by observed hydrogen migration out of the (i-p)a-Si:H stack. However, hydrogen cannot escape from the cell stack, it accumulates near the (p)a-Si:H/ITO contact interface, where ITO acts as a barrier preventing hydrogen loss. Furthermore, light-heat combined stress does not degrade VOC appreciably, confirming the occurrence of a defect annealing process.
DOI: 10.2172/2478089
Authors: Univ. of Delaware, Newark, DE (United States), Ujjwal Das, USDOE Office of Energy Efficiency and Renewable Energy (EERE), Renewable Power Office. Solar Energy Technologies Office, Andrew Teplyakov, Tasnim Mouri, Margaret Zeile, Dhamelyz Rosana Silva Quinones, Tyler Parke, Marissa Piña, John Mason, Noah Jones
Institution: University of Delaware
Language: English
Subfield: Electrical and Electronic Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: green
Awards: IN-SITU HYDROGEN MICROSTRUCTURAL CHARACTERIZATION OF SI HETEROJUNCTION PASSIVATION: ADDRESSING VOC DEGRADATION AND MITIGATION PATHWAYS
THE OVERALL OBJECTIVE OF THE PROJECT IS TO DEVELOP AN IN-SITU CHARACTERIZATION METHOD TO DECIPHER AND QUANTIFY HYDROGEN MICROSTRUCTURAL CHANGES OF HYDROGENATED AMORPHOUS SILICON (A-SI:H)-PASSIVATED CRYSTALLINE SI SURFACE DURING EXPOSURE TO LIGHT AND HEAT UNDER DIFFERENT AMBIENT CONDITIONS. RECORD OPEN CIRCUIT VOLTAGE (VOC) IN SI HETEROJUNCTION (SHJ) SOLAR CELL IS ATTRIBUTED TO THE EXCELLENT SURFACE PASSIVATION OFFERED BY THE INTRINSIC A-SI:H LAYERS. HOWEVER, SUCH SHJ CELLS HAVE EXHIBITED A UNIQUE VOC-DRIVEN PERFORMANCE LOSS TRIGGERED BY COMBINATIONS OF LIGHT, TEMPERATURE, AND VOLTAGE. THESE LOSSES ARE INTERNAL TO THE CELL, RELATED TO THE ELECTRONIC AND STRUCTURAL INSTABILITY OF H-RICH A-SI:H LAYERS AND/OR INTERFACES. THIS PROJECT IN ONE BUDGET PERIOD WILL DEVELOP A FOURIER TRANSFORM INFRARED (FTIR) VIBRATIONAL SPECTROSCOPY BASED QUANTITATIVE ANALYSIS OF HYDROGEN CONCENTRATION AND BONDING STRUCTURES IN THE A-SI:H FILM/INTERFACES, MEASURED IN-SITU DURING LIGHT AND TEMPERATURE STRESSES. THESE IN-SITU MEASURED PARAMETERS WILL BE CORRELATED TO THE EX-SITU MEASURED MINORITY CARRIER LIFETIME (¿EFF), IMPLIED VOC (IVOC) AND CELL VOC UNDER SIMILAR ACCELERATED LIFETIME TESTING (ALT) CONDITIONS. THE FINAL GOALS OF THIS PROJECT ARE TO PROVIDE CRITICAL UNDERSTANDING OF VOC-DRIVEN SHJ CELL PERFORMANCE LOSS MECHANISM AND ESTABLISH A CAUSAL RELATION TO GUIDE DEVELOPMENT OF MITIGATION PATHWAYS., G3135089876
OpenAlex ID: W4404956412