Work

Elucidating the formation mechanism of Zeolite-Templated Carbons

Year: 2023
Type: conference-paper
Abstract: 1.Introduction Zeolite-Templated Carbons are highly microporous and structured carbon materials that seem promising for a wide range of applications such as gas storage and capture, as supercapacitors, and as catalysts.[1] These carbon materials have been described as curved graphene sheets and thereafter, they were claimed to present a Schwarzite structure. This latter assumption has yet strongly been questioned.As indicated by their name, ZTCs correspond to carbon materials achieved through the polymerization of carbon precursors within the microporous system of a sacrificial zeolite template. Despite the large number of zeolite structures identified today (more than 250 structures), only a few of them allow the synthesis of ZTC: *BEA, EMT, and FAU. These three zeolite structures present several common features that appear compulsory for the synthesis of ZTC such as the large pore opening and the tri-dimensionality interconnection of the porous system. Various atomistic structural models have been proposed for ZTCs resulting from the FAU framework based on computational simulation and classified into two main families: open blades and closed struts.[2] On the other hand, carbon structure from *BEA has been described as connected carbon nanotubes or disconnected carbon nanoribbons. Nevertheless, rather little is known about their formation mechanism and the key steps that govern their synthesis. Only few reports have been published that attempt at describing in detail the formation mechanism of ZTCs. The present contribution reports a systematic ex-situ kinetic study of the evolution of the key properties of the developing ZTC using a zeolite with *BEA structure as template. The characterization of chemical, electrical, textural, and morphological properties of hybrids and resulting carbon materials allow to draw a full picture of the ZTC evolution. 2.Experimental part After the synthesis of the template zeolite (beta zeolite, *BEA structure), 1.5 g of the zeolite was placed in a reactor and activated at 150 °C for 1 h and 690 °C for an additional hour under a nitrogen flow. The gas was then switched to a mixture of C2H4 in N2 for the indicated synthesis time (5, 10, 15, 30, 45, 60, 90, 120, 180, and 240 min) and the reactor was cooled to RT under N2. For the experiment 240 min+HT the temperature was raised after 240 min to 890 °C and kept at this temperature for 2 h under N2 flow before cooling to RT. Eleven hybrids (zeolite and carbon species) were obtained. In order to get the final carbon material, a part of each hybrid was treated with hydrofluoric acid, allowing the dissolution of the zeolite. 3.Results The characterization of the hybrids indicates a constant evolution of the textural properties with time. A rapid decrease in the micropore volume is remarked during the first 60 min. The reduction of micropore volume thereafter remains linear yet slower until the complete obstruction after 150 min. The Structural Packing Density (SPD, corresponding to the amount of carbon species per gram of zeolite) increases progressively throughout the synthesis and reaches a maximum value of 0.29 gC/gZ after 240 min. The evolution of the SPD is linear with the reduction of the zeolite micropore volume, indicating that the entirety of the carbonaceous species develops within the zeolite microporosity. It is thus possible to calculate the apparent density of the carbonaceous species that increases strongly and achieves a plateau within 60 min of synthesis. The rapid progress of the apparent density during the first hour of synthesis indicates the important structural evolution of the carbonaceous species that develop within the zeolite microporosity. Apparent density remains constant thereafter, indicating a consistent growth of carbon species. The presence of PAHs could be detected by observing the Raman shift region between 400 and 900 cm-1. Various bands in this Raman shift region indicate the subsistence of a great variety of PAHs. The maximal intensity of the band centered at 590 cm-1 is reached when the zeolite micropore volume is completely occupied and slowly decreases thereafter, indicating a more connected carbon network. Electrical conductivity measurement allows to confirm Raman spectroscopy results. In fact, hybrid materials are electrical insulators during the first hour of synthesis, fostering the suspicion of individual polyaromatic species that develop in the initial stages of the synthesis. The increase of the value of electrical conductivity thereafter indicates the development of sp2 conjugated carbon entities and thus the condensation of PAHs. Electrical conductivity significantly increases as a result of heat treatment. The heat treatment hence reveals as a key step for full condensation of the carbon skeleton. CW-EPR spectroscopy confirms the evolution from a clustered to a homogeneous spin system.After the dissolution of the zeolite, the eleven resulting carbon materials are characterized. Scanning electron microscopy images present unstructured and large carbon agglomerates of undefined morphology achieved for the carbon materials at short syntheses times that do not result from zeolite templating. After one hour, typical morphological features of the zeolite shape start to emerge and only the additional heat treatment allows a perfect replica of the zeolite. This trend is also observable using X-Ray diffraction: the carbon materials achieved after short synthesis times (below 60 min) do not present any XRD peaks related to the structural order of ZTC. Only a broad reflection attributed to the stacking of graphene-like subunits typically observed in unstructured carbons is visible at 24° 2θ. This broad peak starts to disappear after one hour while a new contribution centered at 7.6° 2θ starts to emerge, indicating the beginning of partial long-range order in the carbon materials. Only the subsequent heat treatment allows the presence of a further peak at 15° 2θ, characteristic for ZTCs resulting from beta zeolite featuring high structural quality. Finally, nitrogen physisorption isotherms present open hysteresis loops for all carbons except for the material achieved after heat treatment. This indicates that the carbon backbone is not fully condensed even after complete micropore filling of the zeolite. Only after the heat treatment step, the desorption branch closes the adsorption branch indicating that the material is fully connected. 4.Conclusion The characterization of both hybrid compounds and carbon species after the dissolution of the zeolite, allowed us to conclude that the ZTC formation occurs in three major stages which can be ascribed to nucleation, growth, and condensation. During the stage I, PAHs develop through aromatization of ethylene and growth, catalyzed through the acid sites of the zeolites. Oblong, rylene-type PAHs preferentially develop in the micropores of beta zeolite. The PAHs are of radical nature and react together upon zeolite dissolution, leading to unstructured carbon particles of undefined morphology and random textural properties. This stage was observed for syntheses times below 1 h in the applied conditions. During stage II, typical structural, textural, and morphological features of ZTCs start to emerge. The achieved carbon materials can be described as composites of ZTC and randomly reacted PAHs molecules. This stage was first observed after 60 min of synthesis. Finally, the heat treatment permits the final condensation of the ZTC network corresponding to the stage III, leading to a carbon material with textural, morphological, and structural properties directly resulting from the zeolite templating.[3] [1] H. Nishihara, T. Kyotani, Chem. Commun., 2018, 54, 5648.[2] E. E. Taylor, K. Garman, N. P. Stadie, Chem. Mater., 2020, 32, 2742.[3] T. Aumond, I. Batonneau-Gener, Y. Pouilloux, L. Pinard, D. Wisser, M. Moreau, H. Vezin, A. Moissette, A. Sachse, Mater. Today Chem., 2022, 26, 101053.
Source: HAL
Language: English
Field: Chemistry
Open Access status: green
OpenAlex ID: W4407803452
FWCI:
Cites:
Cited by:
Related to: 9