Work

Effect of the Addition of Al-5Ti-0.25C and Annealing on the Mechanical Properties of Open-Cell Al Foams

Year: 2025
Type: article
Abstract: Ti and TiC phases, which serve as refining agents. Open-cell metallic foams were successfully produced using the replication casting technique, with pore sizes ranging from 1.00 to 3.35 mm. For the infiltration process, refined aluminum was used, while unrefined aluminum served as a baseline reference. The resultant foams underwent multiple annealing cycles at 480 °C, with the most refined and homogeneous microstructure observed after 504 h. Comprehensive microstructural characterization was conducted utilizing scanning electron microscopy and optical microscopy. Additionally, uniaxial compression tests were performed to generate stress-strain profiles for the foams, facilitating an assessment of their energy absorption capacity. The findings indicated an enhancement in energy absorption capacity by a factor of 2.4 to 3, which can be attributed to the incorporation of Al-5Ti-0.25C and the subsequent annealing process.
Source: Materials
Language: English
Open Access status: gold
Estimated APC paid: $3,137
OpenAlex ID: W4410138544
FWCI: 0.89
Cites: 26
Cited by: 3
Related to: 10