Thermomechanical behavior of Ti-6Al-4V alloy via hybrid manufacturing with laser metal deposition and friction stir processing
Year: 2025
Type: article
Abstract: This study investigates the hybrid manufacturing process combining laser metal deposition (LMD) and friction stir processing (FSP). To numerically simulate this hybrid process, a thermo-mechanical coupled model for additive and equivalent manufacturing of Ti-6Al-4V alloy was developed using ABAQUS software. The model reveals the evolution of temperature and stress fields and their influence on microstructure regulation. Results indicate that the layer-by-layer deposition in LMD causes the molten pool temperature to rise incrementally from 1866 °C in the first pass to 2321 °C in the 20th pass. Preheating the substrate to 300 °C reduces the cooling rate by 32.5 % (from 1203.12 °C/s to 812.41 °C/s) and promotes a 9.4 % increase in grain coarsening within the deposited layer. As-deposited components exhibit a stress distribution characterized by tensile stress at the center and compressive stress at the edges, with an average equivalent stress of 650.25 MPa. The FSP process generates a bowl-shaped temperature field of 1380.15 °C in the stirred region, inducing dynamic recrystallization that refines grains by 90.6 % and redistributes stresses to form an “M”-shaped residual stress field (average equivalent stress 251.03 MPa). This model successfully quantifies the thermo-mechanical behavior of the entire hybrid manufacturing process, providing a theoretical foundation for collaborative multi-process regulation of microstructure and properties.
Source: Applied Thermal Engineering
Authors: Kai Zhang, Runze Zhao, Jifei Lv, Fei Xing, Xingyu Jiang, Wenchao Xi, Zhuangzhuang Hou, Weijun Liu
Institution: Shenyang University of Technology
Language: English
Subfield: Mechanical Engineering
Field: Engineering
Domain: Physical Sciences
Open Access status: hybrid
Estimated APC paid: $3,660
Awards: G2875742782, G8897180088
OpenAlex ID: W4410720516