Experimental study on the mechanical properties of GFRP bolts: Insights from failure modes and adhesion strength of the rod-grout interface
Year: 2025
Type: article
Abstract: In underground float-resisting engineering, glass fiber reinforced polymer (GFRP) bolts are becoming more and more popular as substitutes for conventional steel float-resisting bolts due to their superior mechanical properties and corrosion resistance. The differences in failure modes between GFRP and steel float-resisting bolts, ultimate loads, and bond-slip curves were explained in this paper using full-scale destructive pull-outs. It also demonstrates how various influencing factors affected the adhesion strength at the rod-grout interface of GFRP float-resisting bolts. The results indicated that shear slip and bolt fracture were the predominant failure modes for both GFRP and steel float-resisting bolts. Compared to steel float-resisting bolts of the same specifications, the failure loads of GFRP float-resisting bolts with anchorage lengths of 4.5 m and 6.5 m were 21% and 14% higher, respectively. Compared to steel float-resisting bolts, the adhesive properties at the rod-grout interface of GFRP float-resisting bolt were superior. Anchorage length, bolt material, and bolt diameter are key variables, listed in descending order of influence, determining the adhesion strength at the rod-grout interface of float-resisting bolts. Steel float-resisting bolts with longer anchorage lengths and greater bolt diameters may be replaced by GFRP float-resisting bolts with shorter anchorage lengths and smaller bolt diameters.
Language: English
Subfield: Building and Construction
Field: Engineering
Domain: Physical Sciences
Open Access status: gold
Estimated APC paid: $2,660
OpenAlex ID: W4412664910