Correlation between ball milling conditions of powders and mechanical properties of dense nickel prepared by SPS

Year: 2026
Type: article
Abstract: The relationship between fine microstructures and mechanical properties of dense nickel prepared by Spark Plasma Sintering is investigated. Large-sized samples with a diameter of 85 mm and a height of 10mm were sintered using different mechanically activated powders. Two types of tools (WC-Co and graphite) were used to study the both influence of the sintering temperature and the pressure on the mechanical properties of sintered materials. With the use of WC-Co tools, the sintering temperature was 560 °C by applying a uniaxial stress of 155 MPa. For conventional graphite carbon tools, the sintering temperature was 700 °C with a uniaxial stress of 75 MPa. In one hand, higher electrical and thermal conductivities of graphite carbon compared to WC-Co allows to apply a higher heating rate, favoring the densification mechanisms. In another hand, lower sintering temperature with the WC-Co tools leads to limit the grain growth and, consequently, maintaining the crystallite size obtained during the ball milling process. A study on the milling conditions reveals that the increase of the milling energy enables to lower the crystallite size from 92 to 49 nm and to introduce some structural defects. The mechanisms of powder deformation in High-Energy Ball Milling as well as the modification of the sintering conditions (i.e. reduces sintering temperature) influence the dislocation density within the sintered samples. An excellent agreement is observed between microstrain, dislocation density and necking instability of nickel polycrystals with grain sizes varied from sub-micrometers to twenty micrometers.
Language: English
Open Access status: gold
Estimated APC paid: $1,530
OpenAlex ID: W4414754532
FWCI:
Cites: 37
Cited by:
Related to: 10